JFoam™ BX-650 is a two component rigid polyurethane foam system designed for structural void filling applications. This system is well suited for RTM applications where high compressive and tensile strength properties are required during post curing of composite part. BX-650 has a recommended service temperature of 225°F.Information provided by J6 Polymers LLC |