MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Nymax™ 603 SN White Nylon 6 Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: The Nymax® 600 Blend Series of nylon 6 materials are "salt-and-pepper" pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.

Property data measured on molded test bars: Dry as Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 1.5 %
@Thickness 3.18 mm,
Time 86400 sec
1.5 %
@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 78.6 MPa11400 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 45 %45 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.76 GPa400 ksiASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.00 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
@Thickness 3.18 mm
131 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Descriptive Properties
AppearanceWhite
FeaturesGeneral Purpose
FormsPellets
Generic NamePolyamide 6 Alloy (Nylon 6 Alloy)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shakespeare WonderThread® SN-40 ultra soft TEX# 14 Nylon Industrial Sewing Thread
Covestro DESMODURE® PL 340 BA/SN Polyurethane
Covestro DESMODURE® N 3390A BA/SN Polyurethane
Covestro DESMODURE® N 3368A BA/SN Polyurethane
Covestro Desmodur® Z 4470 SN/BA Polyurethane

PH1PN9287 / 103123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.