MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMODURE® PL 340 BA/SN Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Blocked aliphatic polyisocyanate based on IPDI. In combination with polyol components for the formulation of lightfast one-component polyurethane stoving coatings.

Properties / Applications: Desmodur® PL 340 can be combined with suitable, preferably flexible, Desmophen® grades to formulate one-component polyurethane stoving coatings which are lightfast and resistant to weathering and chemicals and highly resistant to thermal yellowing. These coatings are used for original automotive topcoats. Compared with polyisocyanates blocked with butanone oxime, Desmodur® PL 340 allows a reduction in stoving temperature of approx. 10 °C, with no decrease in solvent and chemical resistance.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccDIN 51 757
Volatiles 38 - 42 %38 - 42 %0.2 g / 60 min / 125°C; DIN EN ISO 3251
Viscosity 550 - 650 cP550 - 650 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesMetricEnglishComments
Flash Point 38.0 °C100 °FDIN EN ISO 13 736
 
Descriptive Properties
Color<100DIN EN 1557
Content0.073Blocked NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODURE® N 3368A BA/SN Polyurethane
Covestro DESMODURE® N 3390A BA/SN Polyurethane
Covestro Desmodur® L 67 MPA/X Polyurethane
Covestro Desmodur® L 67 BA Polyurethane
Covestro Desmodur® L 75 Polyurethane

PCOVEST0565 / 202348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.