MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper nickel 20%, UNS C71000, OSO50 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Good hot and cold workability. Fabricated by blanking, forming, and bending.

Applications: communication relays, condensers, condenser plates, electrical springs, evaporator and heat exchanger tubes, ferrules, resistors.

Test specimen: flat products - 1mm thickness.

Key Words: CDA 710 (80/20); 80-20 Cupronickel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 25
Hardness, Rockwell F 72
Tensile Strength, Ultimate 350 MPa
Tensile Strength, Yield 90.0 MPa
@Strain 0.2 %
 90.0 MPa
@Strain 0.5 %
Elongation at Break 35 %in 50 mm
Modulus of Elasticity 140 GPa
Poissons Ratio 0.35Calculated
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 52.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000265 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.4 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 36.0 W/m-K
Melting Point 1150 - 1200 °C
Solidus 1150 °C
Liquidus 1200 °C
Annealing Point 1200 - 1500 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 650 - 825 °C
Hot-Working Temperature 875 - 1050 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 79 %
Iron, Fe <= 1.0 %
Lead, Pb <= 0.050 %
Manganese, Mn <= 1.0 %
Nickel, Ni 19 - 23 %
Other, total <= 0.50 %
Zinc, Zn <= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper nickel 20%, UNS C71000
Copper nickel 10%, UNS C70600
316 Stainless Steel, annealed sheet
304 Stainless Steel
Copper nickel 20%, UNS C71000, H01 Temper flat products

MC71000b2 / 11731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.