MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper nickel 20%, UNS C71000, H01 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Good hot and cold workability. Fabricated by blanking, forming, and bending.

Applications: communication relays, condensers, condenser plates, electrical springs, evaporator and heat exchanger tubes, ferrules, resistors..

Test specimen: flat products - 1mm thickness.

Key Words: CDA 710 (80/20); 80-20 Cupronickel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 5858
Hardness, Rockwell F 9292
Tensile Strength, Ultimate 415 MPa60200 psi
Tensile Strength, Yield  330 MPa
@Strain 0.5 %
47900 psi
@Strain 0.5 %
 338 MPa
@Strain 0.2 %
49000 psi
@Strain 0.2 %
Elongation at Break 20 %20 %in 50 mm
Modulus of Elasticity 140 GPa20300 ksi
Poissons Ratio 0.350.35Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 52.0 GPa7540 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000265 ohm-cm
@Temperature 20.0 °C
0.0000265 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.4 µm/m-°C
@Temperature 20.0 - 300 °C
9.11 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 36.0 W/m-K250 BTU-in/hr-ft²-°F
Melting Point 1150 - 1200 °C2100 - 2190 °F
Solidus 1150 °C2100 °F
Liquidus 1200 °C2190 °F
Annealing Point 649 - 816 °C1200 - 1500 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 650 - 825 °C1200 - 1520 °F
Hot-Working Temperature 875 - 1050 °C1610 - 1920 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 79 %79 %
Iron, Fe <= 1.0 %<= 1.0 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 19 - 23 %19 - 23 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper nickel 20%, UNS C71000
Copper nickel 20%, UNS C71000, H02 Temper flat products
Copper nickel 20%, UNS C71000, H04 Temper flat products
Copper nickel 20%, UNS C71000, H55 Temper flat products
Copper nickel 20%, UNS C71000, OSO50 Temper flat products

MC71000b5 / 11734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.