MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LEXAN™ Copolymer EXL1444 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-40°C) ductility, exhibits excellent processability and release with opportunities for shorter IM cycle times compared to standard PC. Lexan EXL1444 resin is a product available in wide range of opaque colors and may be an excellent candidate for a wide variety of food contact applications.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.150 %0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %0.35 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
9.0 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inSABIC method
 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 8989ASTM D785
Hardness, Rockwell R 121121ASTM D785
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ASTM D638
 60.0 MPa8700 psi50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ASTM D638
 57.0 MPa8270 psi50 mm/min; ISO 527
Elongation at Break 98 %98 %50 mm/min; ASTM D638
 120 %120 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.02 GPa293 ksi50 mm/min; ASTM D638
 2.15 GPa312 ksi1 mm/min; ISO 527
Flexural Strength 85.0 MPa12300 psiyield, 2 mm/min; ISO 178
 92.0 MPa13300 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.23 GPa323 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.25 GPa326 ksi2 mm/min; ISO 178
Izod Impact Notched 865 J638 ft-lbASTM D256
 775 J
@Temperature -30.0 °C
572 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²33.3 ft-lb/in²80*10*3; ISO 180/1A
 60.0 kJ/m²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 J/cm²33.3 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 70.0 J51.6 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant  2.64
@Frequency 1e+6 Hz
2.64
@Frequency 1e+6 Hz
ASTM D150
 2.68
@Frequency 100 Hz
2.68
@Frequency 100 Hz
ASTM D150
Dielectric Strength 16.3 kV/mm
@Thickness 0.800 mm
414 kV/in
@Thickness 0.0315 in
in oil; ASTM D149
Dissipation Factor  0.0012
@Frequency 100 Hz
0.0012
@Frequency 100 Hz
ASTM D150
 0.0093
@Frequency 1e+6 Hz
0.0093
@Frequency 1e+6 Hz
ASTM D150
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.700 mm
>= 120 sec
@Thickness >=0.0276 in
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=0.700 mm
60 - 120 arcs
@Thickness >=0.0276 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  69.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
40.0 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
40.0 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
 74.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 140 °C
@Thickness 3.20 mm
284 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 124 °C
@Thickness 3.20 mm
255 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 145 °C293 °FRate B/50; ISO 306
 145 °C293 °FRate B/50; ASTM D1525
 146 °C295 °FRate B/120; ISO 306
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94 HB
@Thickness >=0.700 mm
HB
@Thickness >=0.0276 in
UL 94
Oxygen Index 37 %37 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80177 / 288124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.