MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton A1536 H is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified:
Kraton A1536 HU - supplied to customers as an undusted powder
Kraton A1536 HS - supplied to customers as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton A1536 H is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens.

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %KM 04
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
Ash 0.35 - 0.70 %Silica dusted; BAM 908
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65
@Time 10.0 sec
Measured on compression molded slabs; ASTM D2240
Tensile Strength >= 34.5 MPaMeasured on solution cast film from toluene; BAM 1245
Elongation at Break >= 660 %Measured on solution cast film from toluene; BAM 1245
300% Modulus 0.00645 GPa
@Strain 300 %
Measured on solution cast film from toluene; BAM 1245
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.07-0.13%, KM 08
 Polystyrene37-44%, Measured on the polymer before hydrogenation, KM 03
 Total Extractables<1.6%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® D1161 J (SIS) Linear Triblock Copolymer
Kraton® G1701 M (SEP) Linear Diblock Copolymer
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer

PKRA9883 / 132782

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.