MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® G1701 M (SEP) Linear Diblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1701 M is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form identified:
Kraton G1701 MU - supplied as a powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1701 M is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Packaging and Polymod; Personal Care; and Medical

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D4025
Volatiles <= 1.0 %<= 1.0 %KM 04
Kinematic Viscosity at 100°C (212°F) 15 - 19 cSt15 - 19 cSt1.7%, ENJ404; BAM 1201
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
<= 1.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Chemical PropertiesMetricEnglishComments
Diblock Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 64
@Time 10.0 sec
64
@Time 0.00278 hour
ASTM D2240
Tensile Strength 2.07 MPa300 psiASTM D412
Elongation at Break 100 %100 %ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.03-0.2%, KM 08
 Polystyrene34.7-38.5%, Measured on the polymer before hydrogenation, KM 03
 Total Extractables<3.0%, KM 05
Styrene/Rubber Ratio37/63

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® G1641 H (SEBS) Linear Triblock Copolymer
Kraton® G1651 E (SEBS) Linear Triblock Copolymer

PKRA9903 / 132802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.