MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Danquinsa EMULTROL® E-58 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: EMULTROL E-58 is a tackifier emulsion. It modifies the adhesivity and cohesion qualities of self-adhesives and adhesives based on water dispersions with acrylic resin, latex, EVA and polyurethane. Its main function is to improve the cohesion on these polymers with no significant effects upon tack. This product has a good wetting on silicone paper and is highly stabilized against ageing and oxidation. The product is even UV proof. EMULTROL E-58 is made of very fine particles, thus avoiding scratching the application cylinders and maintaining product stability during storage.

Application: The resin emulsion acts as modification component in one and two component aqueous adhesive and adhesive coating systems. This emulsion is added to different based aqueous plastic dispersions to achieve a permanent adhesiveness on bonding surfaces of the films. It is used as well to achieve a long open time. A typical application for this emulsion is for example the modification of aqueous primer dispersion adhesives for the coating of adhesive stripes, labels and film materials. We can specially recommend you EMULTROL E-58 for adhesives, where it must be given a high hydrolysis and ageing resistance.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 - 1.03 g/cc
pH 6.5 - 8.5
Viscosity <= 3000 cPRV8, Spindle 3, 50 rpm
Storage Temperature 10.0 - 25.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 20[mg KOH/g], residium
 
Thermal PropertiesOriginal ValueComments
Boiling Point 100 °C
Softening Point 63.0 - 73.0 °CResidue soft point
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Active matter contents49-51%
AspectWhitish liquid
CompositionHydrogenated hydrocarbon resin dispersion.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ171 / 294591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.