MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Global EPP PA 612 Copolymer Cast Polyamide 612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of cast nylons may be altered to suit specific applications, and the performance of the basic polymer can be enhanced with the addition of various additives, fillers, lubricants and colorants.

Key characteristics:

  • Unequalled formulation options and profile range
  • Excellent mechanical, thermal and chemical resistance
  • Excellent PV and load bearing capabilities
  • Excellent wear and abrasion resistance
  • Good dimensional stability, largely free from internal stresses
  • FDA compliant grades available

CP612 is a copolymer of nylon 6 and nylon 12 produced by anionic polymerisation of caprolactam and laurinlactam. The copolymer makeup gives the product a greater degree of material resilience, reduces moisture absorption and greatly improves impact resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccTest Method A; ISO 1183:1987
Water Absorption 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
Immersion; ISO 62:1999 (modified)
Water Absorption at Saturation 5.0 %ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ISO 868:2003
Tensile Strength at Break 75.0 MPaSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 30 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 3.70 GPaSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 95.0 MPa1.5 mm/min; ISO 178:2001
Flexural Modulus 2700 MPa1.5 mm/min; ISO 178:2001
Compressive Strength 90.0 MPaSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 2000 MPaSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 6.50 kJ/m²Sample Type A; ISO 180:2000
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mmIEC 60243-1:1998-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Melting Point 215 °C
Maximum Service Temperature, Air 100 °CContinuous
 160 °CIntermittent
Minimum Service Temperature, Air -100 °CIntermittent
 -40.0 °CContinuous
Flammability, UL94 HBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorNatural, Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global EPP PA 6C Cast Polyamide 6
Nylene® 826 Nylon Copolymer
Nylene® CX3395 Nylon Copolymer
Overview of materials for Nylon 610
Nylene® 8100 Unfilled Nylon 6/12

PGLOEPP08 / 79519

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.