MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Edinburg Plastics BTA706 PBT, Impact Modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Appearance: Lawn & Garden Colors

Processing Methods: Injection

Applications: Hi Impact-Cold Temperature

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792-91
Linear Mold Shrinkage 0.020 - 0.027 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5800 psiASTM D638
Elongation at Break 140 %ASTM D638
Flexural Yield Strength 8400 psiASTM D790
Flexural Modulus 270000 psiASTM D790
Izod Impact, Notched 17.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 232 - 249 °C
Middle Barrel Temperature 243 - 260 °C
Front Barrel Temperature 249 - 266 °C
Nozzle Temperature 243 - 260 °C
Melt Temperature 257 °C
Mold Temperature 49.0 - 77.0 °C
Drying Temperature 121 °C
Dry Time 3.00 - 12.0 hour
Moisture Content <= 0.20 %
Dew Point >= -40.0 °F
Back Pressure 50.0 - 100 psiLower is better
Screw Speed 50 - 100 rpmLower is better

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecodur® PB70 GR30 NL100 IL PBT, 30% glass fiber reinforced, impact modified, natural
Celanese Crastin® S610SF BK851 Polybutylene Terephthalate (PBT)
Edinburg Plastics BGA606 PBT
DuPont Mobility and Materials Crastin® CE2061 BK560 PBT
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT

PEDIN041 / 183544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.