MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Crastin® S610SF BK851 Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production

Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable fo

Former DuPont product acquired by Celanese in 2022.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm0.017 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4, 2577
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 250 °C
50 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-1/-2
Elongation at Break 13 %13 %Nominal; ISO 527-1/-2
Elongation at Yield 10 %10 %ISO 527-1/-2
Tensile Modulus 2.60 GPa377 ksiISO 527-1/-2
Poissons Ratio 0.380.38
Charpy Impact, Notched 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 224 °C435 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Glass Transition Temp, Tg 55.0 °C131 °F10°C/min; ISO 11357-1/-2
Flame Spread 24.0 mm/min
@Thickness 1.00 mm
0.945 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FOptimum, Injection
 235 - 260 °C455 - 500 °FRange, Injection
Mold Temperature 80.0 °C176 °FOptimum, Injection
 30.0 - 130 °C86.0 - 266 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.040 %<= 0.040 %Injection
Hold Pressure >= 60.0 MPa>= 8700 psiInjection
 
Descriptive Properties
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0G-value (condensate); ISO 6452
Part Marking Code>PBT<ISO 11469
PolymerPBT
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPBTISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Edinburg Plastics BGA606 PBT
Celanese Crastin® CE2055 BK580 Polybutylene Terephthalate (PBT)
Celanese Crastin® CE2055 NC010 Polybutylene Terephthalate (PBT)
Celanese Crastin® FGS600F40 NC010 PBT
DuPont Mobility and Materials Crastin® S600LF NC010 PBT

PDSY5045 / 160887

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.