MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Isopropylamine, C3H9N
Categories: Fluid; Solvent

Key Words: C3H9N
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.688 g/cc
@Temperature 20.0 °C
0.0249 lb/in³
@Temperature 68.0 °F
Viscosity 0.381 cP
@Temperature 20.0 °C
0.381 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 59.112 g/mol59.112 g/mol
Vapor Pressure 0.629157 bar
@Temperature 20.0 °C
471.908 torr
@Temperature 68.0 °F
Surface Tension 16.8 dynes/cm
@Temperature 20.0 °C
16.8 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 50.7 bar38000 torr
Critical Temperature 203 °C397 °F
Critical Density 0.258 g/cc0.00932 lb/in³
Critical Molar Volume 229 cm³/mol14.0 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 460.1 J/g197.9 BTU/lb
Specific Heat Capacity 1.591 J/g-°C
@Temperature 25.0 °C
0.3803 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1382 W/m-K
@Temperature 20.0 °C
0.9591 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -95.3 °C-140 °F
Boiling Point 32.5 °C90.5 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.374
@Wavelength 589.3 nm
1.374
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.3637
Antoine's Vapor Pressure B Parameter2582.35
Antoine's Vapor Pressure C Parameter-40.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)75-31-0
Chemical FormulaC3H9N
Critical Compressibility (Zc)0.29
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A1139.7
Dynamic Viscosity Parameter B323.44
Henry's Law Constant (atm m3/mol)7.64E-05
Molar Heat Capacity (298K)94.038 J/mol-K
Molar Heat Capacity of Vapor a Parameter-7.481
Molar Heat Capacity of Vapor b Parameter0.4173
Molar Heat Capacity of Vapor c Parameter-0.0002824
Molar Heat Capacity of Vapor d Parameter8.343E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1221

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Methanethiol (Methyl mercaptan), CH3HS
LG Chemical LGflex TINTM Plasticizer
Isopropyl chloride
Hydrazoic Acid, HN3
Honeywell Dichloromethane

VORGS206 / 99573

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.