MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical LGflex TINTM Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Features: New plasticizer is required high heat-resistance and weatherability because it is strengthen of UL standard. LGflex TINTM is excellent ins higher heat-resistance and weatherability than commercialized production.

Application: UL 105 °C Wire, Migration Resistance Wire & Sheet and Cable

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 270 cP
@Temperature 20.0 °C
270 cP
@Temperature 68.0 °F
Molecular Weight 588 g/mol588 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10
@Treatment Temp. 125 °C,
Time 10800 sec
<= 0.10
@Treatment Temp. 257 °F,
Time 3.00 hour
After Heating, KOH mg/g; JIS K6751
 
Thermal PropertiesMetricEnglishComments
Melting Point -33.0 °C-27.4 °FFreezing Point
Boiling Point 33.0 °C
@Pressure 0.000667 MPa
91.4 °F
@Pressure 0.0967 psi
 
Descriptive Properties
Acidity<0.1 KOH mg/gJIS K6751
Color<30 APHAJIS K6751

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Methyl Ethyl Ketone (CH3CH2COCH3; 2-Butanone; MEK)
3M Novec™ 7000 Engineered Fluid
Shandong Dongyue Shenzhou New Material Co Perfluoropropylenevinylether (PPVE)
ExxonMobil Jayflex™ DINP Plasticizer (Asian Grade)
ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade)

PLAY253 / 148263

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.