MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta RT509F Melamine Fiber Glass Laminate Tube, NEMA G-9
Categories: Polymer; Thermoset; Melamine

Material Notes: Grade RT509 has good electrical properties under humid conditions and excellent arc resistance. Typical applications include fuse tubes and switchboard insulation. RT509 also complies with MIL-I-24768/1, Type GME and ASTM D709 Type IV Grade G-9.

Information provided by Norplex-Micarta

Key Words: Fiber Glass, Micarta, Melamine, NEMA G-9, MIL-I-24768/1 Type GME, ASTM D709 Type IV Grade G-9
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 g/cc0.750" X 1.000"; ASTM D792
Moisture Absorption 0.900 %0.750" X 1.000"; ASTM D570 Condition D1-24/23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 1200.750" X 1.000"; ASTM D785
Tensile Strength 26500 psi0.750" X 1.000"; ASTM D638 Condition A
Compressive Strength 31250 psi0.750" X 1.000"; ASTM D695 Condition A
Compressive Modulus 600 ksi0.750" X 1.000"; ASTM D695 Condition A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 335 V/mil0.750" X 1.000"; ASTM D149 Condition D-48/50
 380 V/mil0.750" X 1.000"; ASTM D149 Condition A
Dielectric Breakdown 40000 V0.750" X 1.000"; ASTM D149 Condition D-48/50
 70000 V0.750" X 1.000"; ASTM D149 Condition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 150 °C0.750" X 1.000"; UL Bulletin 746b
UL RTI, Mechanical with Impact 150 °C0.750" X 1.000"; UL Bulletin 746b
Flammability, UL94 V-00.750" X 1.000"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta MC511AF Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511FR Epoxy Glass Laminate Sheet, NEMA FR-5
Norplex-Micarta NP511 Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta NP600 Phenolic Paper Laminate Sheet

PNORPM136 / 192875

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.