MC511FR is a high strength, medium weave glass epoxy laminate that retains a minimum of 50 percent of its room temperature flexural strength when tested at 150ºC. Typical applications include structural applications when used in elevated temperatures. MC511FR also complies with MIL-I-24768/28, Type GEB-F.Information provided by Norplex-Micarta |
Glass Fiber, Epoxy, Micarta, NEMA FR-5, ASTM D709 Type IV Grade FR-5, MIL-I-24768/28 GEB-F |