MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Saint-Gobain FibreComp® Performance Polyimide/Graphite+Carbon Fiber BMC
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: FibreComp is used for high speed, medium load, low impact applications

Information provided by Saint-Gobain HyComp LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/cc
Water Absorption <= 0.50 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8000 psi
@Temperature 260 °C
 12000 psi
@Temperature 22.8 °C
Tensile Modulus 1600 ksi
@Temperature 260 °C
 2300 ksi
@Temperature 22.8 °C
Flexural Strength 12000 psi
@Temperature 260 °C
 15000 psi
@Temperature 22.8 °C
Flexural Modulus 1500 ksi
@Temperature 260 °C
 2100 ksi
@Temperature 22.8 °C
Compressive Strength 25000 psi
@Temperature 260 °C
 36000 psi
@Temperature 22.8 °C
Izod Impact, Notched 3.00 ft-lb/in
@Temperature 22.8 °C
Coefficient of Friction 0.10 - 0.20
Limiting Pressure Velocity 120000 psi-ft/minUnlubricated
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µin/in-°F
CTE, linear, Transverse to Flow 10.0 µin/in-°F
Maximum Service Temperature, Air 600 °F
Minimum Service Temperature, Air -70.0 °F
 
Descriptive Properties
AlcoholsRecommended
Dilute AcidsRecommended
HydrocarbonsRecommended
Sea WaterRecommended
Strong Bases (pH > 10)Not Recommended
Weak AcidsRecommended

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTGQ884 / 291405

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.