MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Saint-Gobain FibreComp® Performance Polyimide/Graphite+Carbon Fiber BMC
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: FibreComp is used for high speed, medium load, low impact applications

Information provided by Saint-Gobain HyComp LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/cc
Water Absorption <= 0.50 %<= 0.50 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  55.2 MPa
@Temperature 260 °C
8000 psi
@Temperature 500 °F
 82.7 MPa
@Temperature 22.8 °C
12000 psi
@Temperature 73.0 °F
Tensile Modulus  11.0 GPa
@Temperature 260 °C
1600 ksi
@Temperature 500 °F
 15.9 GPa
@Temperature 22.8 °C
2300 ksi
@Temperature 73.0 °F
Flexural Strength  82.7 MPa
@Temperature 260 °C
12000 psi
@Temperature 500 °F
 103 MPa
@Temperature 22.8 °C
15000 psi
@Temperature 73.0 °F
Flexural Modulus  10.3 GPa
@Temperature 260 °C
1500 ksi
@Temperature 500 °F
 14.5 GPa
@Temperature 22.8 °C
2100 ksi
@Temperature 73.0 °F
Compressive Strength  172 MPa
@Temperature 260 °C
25000 psi
@Temperature 500 °F
 248 MPa
@Temperature 22.8 °C
36000 psi
@Temperature 73.0 °F
Izod Impact, Notched 1.60 J/cm
@Temperature 22.8 °C
3.00 ft-lb/in
@Temperature 73.0 °F
Coefficient of Friction 0.10 - 0.200.10 - 0.20
Limiting Pressure Velocity 4.20 MPa-m/sec120000 psi-ft/minUnlubricated
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°F
CTE, linear, Transverse to Flow 18.0 µm/m-°C10.0 µin/in-°F
Maximum Service Temperature, Air 316 °C600 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Descriptive Properties
AlcoholsRecommended
Dilute AcidsRecommended
HydrocarbonsRecommended
Sea WaterRecommended
Strong Bases (pH > 10)Not Recommended
Weak AcidsRecommended

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQ884 / 291405

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.