MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Isoplast® 101 LGF40 Engineering Thermoplastic Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Isoplast® 101 LGF40 ETP is an engineering thermoplastic resin.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.28 MPa186 psiASTM D 638
Tensile Strength, Yield 186 MPa27000 psiASTM D 638
Elongation at Break 2.0 %2.0 %ASTM D 638
Elongation at Yield 2.0 %2.0 %ASTM D 638
Tensile Modulus 12.0 GPa1740 ksiASTM D 638
Flexural Strength 310 MPa45000 psiASTM D 790
Flexural Modulus 10.0 GPa1450 ksiASTM D 790
Izod Impact, Notched  4.27 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
8.00 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D 256
 4.27 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
8.00 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D 256
Dart Drop, Total Energy  17.0 J
@Temperature -29.0 °C
12.5 ft-lb
@Temperature -20.2 °F
ASTM D 3763
 31.0 J
@Temperature 23.0 °C
22.9 ft-lb
@Temperature 73.4 °F
ASTM D 3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C7.78 µin/in-°FASTM D 696
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °Funannealed; ASTM D 648
 210 °C410 °Fannealed; ASTM D 648
Vicat Softening Point 186 °C367 °FASTM D 1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 238 - 260 °C460 - 500 °F
Mold Temperature 66.0 - 88.0 °C151 - 190 °F
Drying Temperature 82.0 - 99.0 °C180 - 210 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF40 - ETPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin
Geon® Performance Solutions Vinyl Flexible 83700 Polyvinyl Chloride, Flexible

PLUBR5031 / 238901

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.