MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Flexible 83700 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Automotive OEM approval(s).

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Volatiles 1.1 %
@Thickness 1.91 mm,
Temperature 105 °C
1.1 %
@Thickness 0.0752 in,
Temperature 221 °F
Loss; Method A; ASTM D1203B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 838315 sec; ASTM D2240
Tensile Strength at Break 15.2 MPa2200 psi510 mm/min; ASTM D638
Elongation at Break 320 %320 %510 mm/min; ASTM D638
Tear Strength 57.9 kN/m330 pliDie C, 2 in/min; ASTM D1004
 
Descriptive Properties
Automotive SpecificationsCHRYSLER MS-DC23 CPN2928 Color: 2850 Black
 CHRYSLER MS-DC232 CPN2865 Color: 2850 Black
 FORD ESB-M4D259 Type IV
 FORD ESB-M4D284 Type IV
 FORD ESB-M4D284-C4 Color: Charcoal, Black
FeaturesGeneral Purpose
 Medium Gloss
FormsPellets
Fungal ResistancePassASTM G21
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Low Temperature FlexibilityPass-29°C, 508.0 µm; 4 hr, 12 mm
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 General Purpose
 Outdoor Applications
Xenon WeatherometerPassSAE J1960; Exterior, 2500 kJ/m², Black, dE*<3.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible D8000 Polyvinyl Chloride, Flexible
Colorite Polymers Flexchem 3551-02 Vinyl Compound
Fainplast Compounds MPH 62/H Medical Flexible PVC, Extrusion
Fainplast Compounds MPH 78 Medical Flexible PVC, Extrusion
Geon® Performance Solutions Vinyl Flexible C9000 Polyvinyl Chloride, Flexible

PH0POL0014 / 144583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.