MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont MOLYKOTE® 55 O-RING GREASE
Categories: Fluid; Lubricant; Silicone Base

Material Notes: Former Dow Corning product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc
@Temperature 25.0 °C
0.960 g/cc
@Temperature 77.0 °F
Kinematic Viscosity 100 cSt100 cSt
 
Mechanical PropertiesMetricEnglishComments
Penetration P(60), 1/10 mm 290290
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
Dropping Point 220 °C428 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month
 
Descriptive Properties
Colorwhite
NLGI Number2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 108 EMULSION
Dow 111 VALVE LUBRICANT & SEALANT
AISI Type O6 Tool Steel
Sinotek Materials Soft Graphite Ring
Mid-Mountain Materials ARMATEX® SRS 28 Silica Fabric Coated with Silicone Rubber

PDOWCO259 / 105960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.