MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type O6 Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: General purpose, oil-hardening, nondeforming alloy tool steel suitable for applications where extreme dimensional accuracy is required. Applications include ring and plug gages, drawing dies, perforating dies and punches where excellent wear resistance is desired. Contains free graphite in the microstructure to improve machinability.

Key Words: AISI Oil-Hardening Tool Steel O6, UNS T31506, ASTM A681, FED QQ-T-570, SAE J437, SAE J438, oil-hardening, non-deforming alloy tool steel suitable, dimensional accuracy, wear resistant, ring gages, plug gages, drawing dies, perforating dies and punches
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.67 g/cc0.277 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 752752Converted from Rockwell C hardness.
Hardness, Knoop 850850Converted from Rockwell C hardness.
Hardness, Rockwell C 6565As hardened, 64.0 HRC at 120°C temper, 63.0 HRC at 150°C temper, 62.0 HRC at 175°C temper, 61 HRC at 190°C and 205°C temper, 60 HRC at 230°C temper, 59.5 HRC at 260°C temper, 58.5 HRC at 315°C temper. Oil quenched from 800°C, tempered for 1 hour.
Hardness, Vickers 819819Converted from Rockwell C hardness.
Bulk Modulus 160 GPa23200 ksiTypical for steels.
Machinability 130 %130 %Based on 100% machinability for 1% carbon tool steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steels.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.48 µm/m-°C
@Temperature 25.0 - 250 °C
6.933 µin/in-°F
@Temperature 77.0 - 482 °F
 12.86 µm/m-°C
@Temperature 25.0 - 300 °C
7.144 µin/in-°F
@Temperature 77.0 - 572 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 315 °C347 - 599 °FTempering Temperature
 790 - 815 °C1450 - 1500 °FHardening Temperature
Annealing Temperature 765 - 790 °C1410 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.25 - 1.55 %1.25 - 1.55 %
Chromium, Cr <= 0.30 %<= 0.30 %
Iron, Fe 96 %96 %As Balance
Manganese, Mn 0.70 %0.70 %
Molybdenum, Mo 0.25 %0.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 1.03 %1.03 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C
AISI Type O7 Tool Steel
AISI Type A2 Tool Steel
AISI Type A6 Tool Steel
AISI Type A7 Tool Steel

MSTO6A / 14104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.