MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Acrel® 730B resins can be continuously or batch expanded using conventional EPS expansion equipment. Some minor material handling modifications may be required. For molded part densities below 24 g/L (1.5 pcf), double-pass pre-expansion is required. Arcel 730B resins have been expanded in continuous expanders ranging in size from 210 to 1,135 liters (55 to 300 gallons) as well as several sizes of batch expanders.

NOVA Chemicals' ARCEL resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0168 g/cc0.000607 lb/in³Continuous - Double Pass, Pre-puff Density
 0.0184 g/cc0.000665 lb/in³Continuous - Double Pass, Foam Density
 0.0216 g/cc0.000780 lb/in³Batch - Single Pass, Pre-puff Density
 0.0224 g/cc0.000809 lb/in³Continuous - Single Pass, Pre-puff Density
 0.0240 g/cc0.000867 lb/in³Batch - Single Pass, Foam Density
 0.0248 g/cc0.000896 lb/in³Continuous - Single Pass, Foam Density
Filler Content 0.30 %0.30 %Plasticizer
 10.5 %10.5 %Pentane
Particle Size 800 - 1700 µm800 - 1700 µmDiameter; 98% of particles
Storage Temperature <= 4.00 °C<= 39.2 °FRaw Bead
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.287 MPa41.6 psi1.25 pcf; ASTM-D3575
 0.338 MPa49.0 psi1.5 pcf; ASTM-D3575
 0.389 MPa56.4 psi1.75 pcf; ASTM-D3575
 0.440 MPa63.8 psi2 pcf; ASTM-D3575
 0.542 MPa78.6 psi2.5 pcf; ASTM-D3575
 0.645 MPa93.5 psi3 pcf; ASTM-D3575
Flexural Strength 0.228 MPa33.0 psiat Max Load; 1.25 pcf; ASTM-C203
 0.289 MPa41.9 psiat Max Load; 1.5 pcf; ASTM-C203
 0.350 MPa50.7 psiat Max Load; 1.75 pcf; ASTM-C203
 0.411 MPa59.6 psiat Max Load; 2 pcf; ASTM-C203
 0.534 MPa77.4 psiat Max Load; 2.5 pcf; ASTM-C203
 0.656 MPa95.2 psiat Max Load; 3 pcf; ASTM-C203
 0.178 MPa
@Strain 5.0 %
25.8 psi
@Strain 5.0 %
1.25 pcf; ASTM-C203
 0.238 MPa
@Strain 5.0 %
34.5 psi
@Strain 5.0 %
1.5 pcf; ASTM-C203
 0.299 MPa
@Strain 5.0 %
43.3 psi
@Strain 5.0 %
1.75 pcf; ASTM-C203
 0.359 MPa
@Strain 5.0 %
52.0 psi
@Strain 5.0 %
2 pcf; ASTM-C203
 0.479 MPa
@Strain 5.0 %
69.5 psi
@Strain 5.0 %
2.5 pcf; ASTM-C203
 0.600 MPa
@Strain 5.0 %
87.0 psi
@Strain 5.0 %
3 pcf; ASTM-C203
Flexural Strain at Break 9.4 %9.4 %Flexural Strain; at Max Load; 3 pcf; ASTM-C203
 10.3 %10.3 %Flexural Strain; at Max Load; 2.5 pcf; ASTM-C203
 11.3 %11.3 %Flexural Strain; at Max Load; 2 pcf; ASTM-C203
 11.7 %11.7 %Flexural Strain; at Max Load; 1.75 pcf; ASTM-C203
 12.2 %12.2 %Flexural Strain; at Max Load; 1.5 pcf; ASTM-C203
 12.7 %12.7 %Flexural Strain; at Max Load; 1.25 pcf; ASTM-C203
Compressive Strength  0.0876 MPa
@Strain 10 %
12.7 psi
@Strain 10 %
1.25 pcf; ASTM-D3575
 0.112 MPa
@Strain 25 %
16.2 psi
@Strain 25 %
1.25 pcf; ASTM-D3575
 0.117 MPa
@Strain 10 %
17.0 psi
@Strain 10 %
1.5 pcf; ASTM-D3575
 0.144 MPa
@Strain 25 %
20.9 psi
@Strain 25 %
1.5 pcf; ASTM-D3575
 0.148 MPa
@Strain 10 %
21.4 psi
@Strain 10 %
1.75 pcf; ASTM-D3575
 0.161 MPa
@Strain 50 %
23.4 psi
@Strain 50 %
1.25 pcf; ASTM-D3575
 0.177 MPa
@Strain 25 %
25.7 psi
@Strain 25 %
1.75 pcf; ASTM-D3575
 0.178 MPa
@Strain 10 %
25.8 psi
@Strain 10 %
2 pcf; ASTM-D3575
 0.198 MPa
@Strain 50 %
28.7 psi
@Strain 50 %
1.5 pcf; ASTM-D3575
 0.210 MPa
@Strain 25 %
30.5 psi
@Strain 25 %
2 pcf; ASTM-D3575
 0.234 MPa
@Strain 50 %
34.0 psi
@Strain 50 %
1.75 pcf; ASTM-D3575
 0.238 MPa
@Strain 10 %
34.5 psi
@Strain 10 %
2.5 pcf; ASTM-D3575
 0.271 MPa
@Strain 50 %
39.3 psi
@Strain 50 %
2 pcf; ASTM-D3575
 0.276 MPa
@Strain 25 %
40.0 psi
@Strain 25 %
2.5 pcf; ASTM-D3575
 0.299 MPa
@Strain 10 %
43.3 psi
@Strain 10 %
3 pcf; ASTM-D3575
 0.341 MPa
@Strain 25 %
49.5 psi
@Strain 25 %
3 pcf; ASTM-D3575
 0.345 MPa
@Strain 50 %
50.0 psi
@Strain 50 %
2.5 pcf; ASTM-D3575
 0.388 MPa
@Strain 75 %
56.3 psi
@Strain 75 %
1.25 pcf; ASTM-D3575
 0.418 MPa
@Strain 50 %
60.6 psi
@Strain 50 %
3 pcf; ASTM-D3575
 0.449 MPa
@Strain 75 %
65.1 psi
@Strain 75 %
1.5 pcf; ASTM-D3575
 0.509 MPa
@Strain 75 %
73.8 psi
@Strain 75 %
1.75 pcf; ASTM-D3575
 0.570 MPa
@Strain 75 %
82.6 psi
@Strain 75 %
2 pcf; ASTM-D3575
 0.6902 MPa
@Strain 75 %
100.1 psi
@Strain 75 %
2.5 pcf; ASTM-D3575
 0.8108 MPa
@Strain 75 %
117.6 psi
@Strain 75 %
3 pcf; ASTM-D3575
Puncture Energy 42.8 J31.6 ft-lbat Max Load; 1.25 pcf; ASTM-D3763
 51.2 J37.8 ft-lbat Max Load; 1.5 pcf; ASTM-D3763
 60.5 J44.6 ft-lbat Max Load; 1.75 pcf; ASTM-D3763
 81.1 J59.8 ft-lbat Max Load; 2 pcf; ASTM-D3763
Tear Strength 1.47 kN/m8.39 pliat max load; 1.25 pcf; ASTM-D3575
 1.81 kN/m10.3 pliat max load; 1.5 pcf; ASTM-D3575
 2.16 kN/m12.3 pliat max load; 1.75 pcf; ASTM-D3575
 2.51 kN/m14.3 pliat max load; 2 pcf; ASTM-D3575
 3.21 kN/m18.3 pliat max load; 2.5 pcf; ASTM-D3575
 3.89 kN/m22.2 pliat max load; 3 pcf; ASTM-D3575
 
Descriptive Properties
ColorWhite/Neutral
ShapeSpherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
Borealis Borstar® FB3450 HDPE for Film Extrusion
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications

PNOVB108 / 194716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.