MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: 100% Polystyrene.

Pre-expansion

This is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry into the future. The unique design of polystyrene chains gives less sensitivity to steam - hence accurate density control over the unique property of S332. The combination of good properties is clearly a result of high technology in combination with extensive product development.

Shape Moulding

The unique design of polystyrene chains adds numerous advantages to Jackocell® S332 in high density shape molding. Fast molding cycles, good fusion, and easy to reach good surface. The additional broad molding window further reduces waste material and maintains a high quality to the extent that it can be recognized long term on productivity and financial earnings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0280 g/cc0.00101 lb/in³1.2 minute residence time pre-expander
 0.0360 g/cc0.00130 lb/in³2 minute residence time pre-expander
 0.0380 g/cc0.00137 lb/in³2.6 minute residence time pre-expander
 0.0960 g/cc0.00347 lb/in³3.6 minute residence time pre-expander
Bead Size 0.600 - 1.00 mm0.0236 - 0.0394 in
 
Chemical PropertiesMetricEnglishComments
Blowing Agent Content <= 4.0 %<= 4.0 %Pentane
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 0.550 MPa79.8 psi30 g/l
 1.05 MPa152 psi50 g/l
 1.60 MPa232 psi70 g/l
 2.05 MPa297 psi90 g/l
Compressive Strength 2.55 MPa370 psi30 g/l
 4.69 MPa680 psi50 g/l
 7.85 MPa1140 psi70 g/l
 10.9 MPa1580 psi90 g/l
 
Descriptive Properties
Coefficient of Variation (%), max15
Molding Cycle Time (sec)23050 g/l, 24 hours @ 18°C
 36070 g/l, 24 hours @ 18°C
 38090 g/l, 24 hours @ 18°C
 6030 g/l, 24 hours @ 18°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer
NOVA Chemicals Expandable Polystyrene (EPS) 33MB Expandable Polystyrene Resin
NOVA Chemicals Expandable Polystyrene (EPS) M77AG Expandable Polystyrene Resin

PJACK005 / 85571

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.