MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Flint Hills AP7710-HS Impact Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: TPO copolymer, UL certified, and FDA compliant.

Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.

Applications: Injection molding: automotive items and exterior equipment components.

Former Huntsman polypropylene products are now produced by Flint Hills Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 10 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 40ASTM D785
Tensile Strength, Yield 19.0 MPaASTM D638
Elongation at Yield 30 %ASTM D638
Flexural Modulus 0.850 GPaTangent; ASTM D790
Gardner Impact >= 36.0 J
@Temperature -30.0 °C
ASTM D3029
Impact Test 23.0 J
@Temperature -30.0 °C
Multi-axial Impact; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Flint Hills AP5135-HS Impact Copolymer Polypropylene
Flint Hills AP5520-HA Polypropylene Impact Copolymer
Flint Hills P6G4Z-097 Impact Copolymer Polypropylene
Flint Hills AP6106-HS Impact Copolymer Polypropylene
Flint Hills AP5995-HA Polypropylene Impact Copolymer

PHUO30 / 47739

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.