MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Flint Hills AP5135-HS Impact Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Medium impact copolymer, FDA compliant

Features: Nucleated and heat stabilized.

Applications: Injection molding: large, thin wall automotive interior parts and housewares.

Former Huntsman polypropylene products are now produced by Flint Hills Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 35 g/10 min35 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus 1.45 GPa210 ksiTangent; ASTM D790
Izod Impact, Notched 0.700 J/cm1.31 ft-lb/in23° C; ASTM D256
Gardner Impact 7.00 J
@Temperature -30.0 °C
5.16 ft-lb
@Temperature -22.0 °F
ASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Flint Hills AP6835-HS Polypropylene Impact Copolymer
Flint Hills AP4135-HS Polypropylene Impact Copolymer
Flint Hills AP7535-HS Polypropylene Ultra High Impact Copolymer
Flint Hills AP5520-HA Polypropylene Impact Copolymer
Flint Hills P6G4Z-097 Impact Copolymer Polypropylene

PHUO22 / 47731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.