MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Northstar Polymers MYP-V40A Polyurethane Filler Gel
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: This polyurethane casting material is developed for applications that require inexpensive liquid resin filler such as encapsulation of a large electric components or puncture-free tire for low-speed wheels such as of wheel barrows and bicycles.

This is a two-part system with a long pot-life. Once you mix part-A and part-B component, it will stay liquid over one hour at room temperature. The material cures to gel consistency in about 4 to 5 hours. The material can be used in service in between overnight and 3 days depending on the physical demand. Because of the long pot life, the required can be mixed in a mixing container then transferred into a low-pressure injection system to inject it into the filling space, such as a tire, from a narrow entrance.

This material is made from bio-base components. About 60% of the material is consisted of soybean oil base chemical. There is an odor associated with the soybean oil based chemical. It is unsuitable for applications this odor will be a problem. Because it is largely consisted of vegetable oil based material, the material is hydrophobic and it prevents entry of moisture after it is cured.

The material is mechanically weak; the cured gel consistency resembles that of “Finger Jell-O”. It can be easily torn by hands. It is ideal for an application to encapsulate an electric component, which requires re-entry for repair or maintenance. If it is used in mechanically demanding application, such as tire-filling, the material needs to be encapsulated in a strong outer structure. The cured hardness is Shore Durometer OO 42.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 86.0 °FPrepolymer Temperature
 68.0 - 86.0 °FCuring Agent Temperature
Mold Temperature 68.0 - 86.0 °F
Cure Time 4.00 - 5.00 hour
@Temperature 25.0 °C
De-mold Time
 24.0 - 72.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 60.0 - 90.0 min
 
Descriptive Properties
Curing AgentYPX-164
PrepolymerMNA-013
Weight Ratio1:15.724Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Sealing Solutions Turcite® TA Self-Lubricating Thermoplastic Rod
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod
Trelleborg Sealing Solutions HiMod® 911 Thermoplastic Bearing
SSAB Tunnplat Docol® 1000 DP High-strength Steel
Saint-Gobain Rulon® LR Bearing/Seal PTFE

PNORTH867 / 162583

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.