MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe LSS™ 2367 Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: TLS 2367 is a chromium-molybdenum hot work steel that is similar to AISI H11 hot work steel, but which contains a higher molybdenum content. The higher molybdenum gives TLS 2367 better hot hardness and temper resistance, along with higher attainable hardness and deeper hardenability than the more common H11 and H13 hot work steels. Typical applications include extrusion tooling, hot forging dies, hot heading dies, hot shear blades, hot punches and mandrels, hot gripper dies, and die casting tooling for copper and brass.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 56Oil Quenched from 1024°C, 45 minutes
 57Oil Quenched from 1080°C, 20 minutes
Machinability 75 - 80 %1% Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.9 µm/m-°C
@Temperature 20.0 - 100 °C
 13.1 µm/m-°C
@Temperature 20.0 - 500 °C
Thermal Conductivity 27.5 W/m-K
@Temperature 700 °C
 32.2 W/m-K
@Temperature 350 °C
 36.4 W/m-K
@Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 850 °CCritical Temperaure Ae1
 853 °CCritical Temperaure Ar1
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.38 %
Chromium, Cr 5.0 %
Iron, Fe 90.22 %
Manganese, Mn 0.45 %
Molybdenum, Mo 3.0 %
Silicon, Si 0.40 %
Vanadium, V 0.55 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel
AISI 1020 Steel, as rolled
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel

NTIMK098 / 19445

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.