MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also available in the special grades ISODISC and ISOBLOC with improved homogeneity and increased toughness.

Applications: Heavy duty hot work tools and dies, mainly for light alloy processing: mandrels, dies and containers for metal tube and rod extrusion; hot extrusion equipment; tools and dies for the manufacture of hollow bodies, screws, rivets, nuts and bolts. Die casting equipment, forming dies, die inserts, hot shear blades, and plastic molding dies.

Key Words: EN 1.2367; X38CrMoV5-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  7.65 g/cc
@Temperature 600 °C
0.276 lb/in³
@Temperature 1110 °F
 7.69 g/cc
@Temperature 500 °C
0.278 lb/in³
@Temperature 932 °F
 7.85 g/cc
@Temperature 20.0 °C
0.284 lb/in³
@Temperature 68.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1100 - 1380 MPa
@Temperature 315 °C
160000 - 200000 psi
@Temperature 599 °F
varies with heat treatment
 1200 - 1590 MPa
@Temperature 20.0 °C
174000 - 231000 psi
@Temperature 68.0 °F
varies with heat treatment
Tensile Strength, Yield  900 - 1170 MPa
@Strain 0.2 %,
Temperature 315 °C
131000 - 170000 psi
@Strain 0.2 %,
Temperature 599 °F
 1000 - 1380 MPa
@Strain 0.2 %,
Temperature 20.0 °C
145000 - 200000 psi
@Strain 0.2 %,
Temperature 68.0 °F
Reduction of Area  50 %
@Temperature 20.0 °C
50 %
@Temperature 68.0 °F
 50 %
@Temperature 315 °C
50 %
@Temperature 599 °F
Modulus of Elasticity  165 GPa
@Temperature 600 °C
23900 ksi
@Temperature 1110 °F
 176 GPa
@Temperature 500 °C
25500 ksi
@Temperature 932 °F
 215 GPa
@Temperature 20.0 °C
31200 ksi
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000500 ohm-cm
@Temperature 20.0 °C
0.0000500 ohm-cm
@Temperature 68.0 °F
 0.0000590 ohm-cm
@Temperature 600 °C
0.0000590 ohm-cm
@Temperature 1110 °F
 0.0000840 ohm-cm
@Temperature 500 °C
0.0000840 ohm-cm
@Temperature 932 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 100 °C
6.39 µin/in-°F
@Temperature 212 °F
 12.0 µm/m-°C
@Temperature 200 °C
6.67 µin/in-°F
@Temperature 392 °F
 12.2 µm/m-°C
@Temperature 300 °C
6.78 µin/in-°F
@Temperature 572 °F
 12.5 µm/m-°C
@Temperature 400 °C
6.94 µin/in-°F
@Temperature 752 °F
 12.9 µm/m-°C
@Temperature 500 °C
7.17 µin/in-°F
@Temperature 932 °F
 13.0 µm/m-°C
@Temperature 600 °C
7.22 µin/in-°F
@Temperature 1110 °F
 13.2 µm/m-°C
@Temperature 700 °C
7.33 µin/in-°F
@Temperature 1290 °F
Specific Heat Capacity  0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
 0.548 J/g-°C
@Temperature 500 °C
0.131 BTU/lb-°F
@Temperature 932 °F
 0.590 J/g-°C
@Temperature 600 °C
0.141 BTU/lb-°F
@Temperature 1110 °F
Thermal Conductivity  28.8 W/m-K
@Temperature 700 °C
200 BTU-in/hr-ft²-°F
@Temperature 1290 °F
Hardened and tempered
 29.0 W/m-K
@Temperature 100 °C
201 BTU-in/hr-ft²-°F
@Temperature 212 °F
Hardened and tempered
 29.2 W/m-K
@Temperature 600 °C
203 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Hardened and tempered
 30.4 W/m-K
@Temperature 500 °C
211 BTU-in/hr-ft²-°F
@Temperature 932 °F
Hardened and tempered
 30.4 W/m-K
@Temperature 200 °C
211 BTU-in/hr-ft²-°F
@Temperature 392 °F
Hardened and tempered
 31.1 W/m-K
@Temperature 300 °C
216 BTU-in/hr-ft²-°F
@Temperature 572 °F
Hardened and tempered
 31.1 W/m-K
@Temperature 400 °C
216 BTU-in/hr-ft²-°F
@Temperature 752 °F
Hardened and tempered
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 %0.38 %
Chromium, Cr 5.0 %5.0 %
Iron, Fe 90.47 %90.47 %As remainder
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 2.8 %2.8 %
Silicon, Si 0.40 %0.40 %
Vanadium, V 0.55 %0.55 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Latrobe LSS™ 2367 Hot Work Tool Steel
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel

NBUCOR68 / 133741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.