MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 412 Clear Electronic Potting Silicone
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: ChemSet 412 Clear Electronic Potting Silicone is a low viscosity, two-component, addition cure, silicone elastomer which cures at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing electrical insulation and shock resistance.

Key Features: Medium viscosity, Fast room temperature cure, Low linear shrinkage, Transparent, UL 94 HB listed, control number: QMFZ2.E205830.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccChem-Set ™ 412A, uncatalyzed
 1.00 g/ccChem-Set ™ 412B, uncatalyzed
Viscosity 4550 cPChem-Set 412A, uncatalyzed
 5200 cPChem-Set 412B, uncatalyzed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
@Temperature 150 °C
cured, 30 minutes
Tensile Strength 650 psicured. 30 minutes @ 150°C
Elongation at Break 150 %Cured 30 minutes @ 150°C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.180 W/m-K
Maximum Service Temperature, Air 392 °FUseful Temperature
Minimum Service Temperature, Air -58.0 °FUseful Temperature
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.40
 
Processing PropertiesOriginal ValueComments
Gel Time 28.0 minmix ratio 1:1 by wt, catalyzed
 
Descriptive Properties
AppearanceChem-Set ™ 412A: Translucent, uncatalyzed
 Chem-Set ™ 412B: Transparent, uncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-BOND® 1038 Conductive Silicone RTV Adhesive
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Fast Cure Silicone Rubber
Dow Q2-7406 ADHESIVE
Dow JCR 6110 A/B
Dow HIPEC® Q3-6645 SEMICONDUCTOR PROTECTIVE COATING KIT

PCHEMI913 / 232192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.