MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Fast Cure Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL™ RTV 1556 is a two component, high strength, addition cure, room temperature or heat vulcanized silicone rubber compound. Designed specifically for moldmaking applications, it offers low viscosity, high tear cut resistance, and easy release for long lasting molds. BLUESIL™ RTV 1556 has high temperature and chemical resistance with excellent flexibility, low shrinkage, and excellent detail reproduction which makes it well suited for production and prototyping use with all types of casting resins.

Applications:

  • Conventional production and prototype molds
  • Giftware, furniture, and artistic molding
  • Finished rubber parts
  • Electronic encapsulation
  • Stereolithography (SLA) molds
  • Epoxy laminate molding
  • Picture frames, mirrors, and furniture molding

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Viscosity 10000 cP10000 cPPart B, Catalyst Component
 12000 cP12000 cPMixed
 15000 cP15000 cPPart A, Base Component
Linear Mold Shrinkage  <= 0.0010 cm/cm
@Time 86400 sec
<= 0.0010 in/in
@Time 24.0 hour
 0.0010 cm/cm
@Time 605000 sec
0.0010 in/in
@Time 168 hour
Storage Temperature 24.0 °C75.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030ASTM D2240
Tensile Strength 7.136 MPa1035 psiASTM D412
Elongation at Break 660 %660 %ASTM D412
Tear Strength 22.8 kN/m130 pliASTM D624, Die B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+14 ohm-cm7.00e+14 ohm-cm
Dielectric Constant 3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
Dielectric Strength 18.1 kV/mm460 kV/in
Dissipation Factor 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 290 µm/m-°C161 µin/in-°F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 249 °C480 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min168 hour50% RH
Pot Life 15.0 min15.0 min
Working Life 30.0 - 60.0 min30.0 - 60.0 min
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
ColorTranslucentPart A, Base Component
 TranslucentPart B, Catalyst Component
Mix Ratio10:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber
Overview of materials for Silicone, RTV, Construction Grade
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
Humiseal 1C49 Silicone Conformal Coating
Elkem (Bluestar Silicones) BLUESIL™ RTV 3165 A&B Silicone Rubber

PBLUST040 / 191016

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.