MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL® RTV 3611 A&B is a two component, 10 durometer, room temperature curable silicone elastomer designed for use in special effects applications, especially where flexibility and repetitive motion is required. It’s superior physical properties and softness also allows use in orthopedic applications.

Applications:

  • Animatronics; special effect skins
  • Props for the film industry
  • Theme park props and reproduction molds
  • Cushioning applications
Features:
  • Translucent – can be pigmented
  • Easy to use
  • Excellent combination of softness and mechanical strength
  • Low viscosity

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccA; TP 013
 1.10 g/cc1.10 g/ccB; TP 013
Viscosity 2500 cP2500 cPA
 2500 cP2500 cPB
Storage Temperature 24.0 °C75.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1010ASTM D2240
Tensile Strength 2.96 MPa430 psiASTM D412
Elongation at Break 800 %800 %ASTM D412
Tear Strength 14.0 kN/m80.0 pliASTM D624, Die B
 
Processing PropertiesMetricEnglishComments
Pot Life 90.0 min90.0 minNM 128
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorTranslucentA
 TransparentB
Mix Ratio1:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Humiseal 1C49 Silicone Conformal Coating
Humiseal 1C51 Silicone Conformal Coating
Humiseal 1C55 Silicone Conformal Coating
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Fast Cure Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber

PBLUST043 / 191019

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.