MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled; Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/cc
Linear Mold Shrinkage, Flow 0.0040 - 0.0065 cm/cm
Linear Mold Shrinkage, Transverse 0.011 - 0.014 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa
Elongation at Break 2.8 %
Tensile Modulus 9700 MPa
Charpy Impact Unnotched 40.0 kJ/m²
Charpy Impact, Notched 8.00 kJ/m²
Coefficient of Friction, Dynamic 0.18
Coefficient of Friction, Static 0.22
K (wear) Factor 22.0 x 10-8 mm³/N-M
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 VA solution
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
Vicat Softening Point 205 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 0.750 mm
Oxygen Index 28 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
Glow Wire Ignition Temperature 725 °C
@Thickness 1.00 mm
 725 °C
@Thickness 2.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 250 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 100 - 120 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled
LG Chemical Lupox® GP2306FB PBT+GF30%

PLATH9887 / 177583

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.