MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 23 materials in the category Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 23 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
 2Mocom (ALBIS) ALCOM® PBT 700/1 GF20 PTFE15 PBT, 20% Glass/15% PTFE Reinforced
 3Mocom (ALBIS) ALCOM® PBT 700/1 GF30 PTFE15 PBT, 30% Glass/15% PTFE Reinforced
 4Mocom (ALBIS) ALCOM® PBT 700/8GF15 PTFE15 PBT, 15% Glass Fiber/15% PTFE Reinforced
 5Mocom (ALBIS) ALCOM® PBT 700/1 GF30 TF15 SI2 PBT, 30% Glass Fibers, 15% PTFE, 2% Silicone Reinforced
 6Mocom (ALBIS) ALCOM® PBT 700/1.5 HR GF15 PTFE15 PBT, 15% Glass Fibers, 15% PTFE Reinforced
 7LyondellBasell LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy
 8Eurotec® Tecodur® PB7 GR15 NL RT PBT, 15% glass fiber reinforced, PTFE modified, natural
 9LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
 10LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
 11DiscontinuedPolymer Resources TP-G30-TFE15 Polybutylene Terephthalate, 30% Glass Reinforced, 15% PTFE
 12RTP Company RTP 1002 TFE 10 Polybutylene Terephthalate (PBT); Glass Fiber - PTFE Lubricated
 13RTP Company RTP 1007 TFE 10 Polybutylene Terephthalate (PBT); Glass Fiber - PTFE Lubricated
 14RTP Company RTP 1005 TFE 15 Polybutylene Terephthalate (PBT), Glass Fiber - PTFE Lubricated
 15RTP Company RTP 1001 TFE 15 Z Polybutylene Terephthalate (PBT), Glass Fiber - PTFE Lubricated - FDA Compliant Ingredients
 16DiscontinuedRTP Company RTP 1003 GB 20 TFE 15  Polybutylene Terephthalate (PBT) Glass Fiber 20% - Glass Bead 20% - PTFE 15%
 17DiscontinuedRTP Company RTP 1001 TFE 15  Polybutylene Terephthalate (PBT) Glass Fiber 10% - PTFE 15%
 18Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE
 19DiscontinuedAlbis Plastics PBT 700/9 GR 25 , 25% Glass, PTFE Added
 20DiscontinuedAlbis Plastics PBT 700/1 GF 30 PTFE 15 SI 2 , 30% Glass, 15%PTFE and 2% Silicon
 21DiscontinuedLNP Lubricomp® WFL-4034 Polybutylene Terephthalate, Glass Fiber Reinforced, PTFE Lubricant
 22DiscontinuedLNP Lubricomp® WFL-4036 Polybutylene Terephthalate, Glass Fiber Reinforced, PTFE Lubricant
 23DiscontinuedLNP Lubricomp® WFL-4036 BK8-115 Polybutylene Terephthalate, Glass Fiber Reinforced, PTFE Lubricant
 
Found 23 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.