MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Bonded Particle Filtration Media
Categories: Ceramic

Material Notes: Bonded particle filtration media is a proven and efficient means for removing oxides from molten aluminum and its alloys. This filtration media is available in either high strength alumina oxide or silicon carbide, and can be supplied in plate, cylindrical and custom shapes.

Applications

  • In-line filtration (filter wall)
  • Dip wells
  • Charge wells
  • Stalk Tubes

Advantages

  • Improves Melt Quality
  • Stronger than ceramic foam filters
  • Easy to install
  • Long service life
  • Thermally conductive

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 - 2.30 g/cc
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1093 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek B-3A REFRACTORY BOARD
Pyrotek EZ-400 Refractory Coating
Pyrotek ISOCAST Insulating Refractory Castable
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Pyrotek ISOMAG® 175 Structural Insulation Board

CPYRO198 / 1915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.