MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Categories: Carbon; Graphite

Material Notes: Isoflow Graphite Rings facilitate an even flow of oil around the circumference of the billet. This even flow results in improved billet surface quality over long casting campaigns. Isoflow Graphite Rings are fabricated using high strength iso-statically pressed graphite that features very uniform pore size and pore distribution.
Average Grain Size: 15 microns

Advantages

  • ISO 9002 Certified

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 - 1.75 g/cc0.0614 - 0.0632 lb/in³
Open Porosity 15 %15 %
Permeability 0.00300.0030Darcys
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 10.5 - 11.2 GPa1520 - 1620 ksi
Flexural Strength 45.0 - 46.5 MPa6530 - 6740 psi
Compressive Strength 89.7 - 91.4 MPa13000 - 13300 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek B-3A REFRACTORY BOARD
Graphite, Carbon, C
Pyrotek Bonded Particle Filtration Media
Pyrotek EZ-400 Refractory Coating
Pyrotek ISOCAST Insulating Refractory Castable

CPYRO196 / 1913

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.