MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 1300A Polyester (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Very high melt flow

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccASTM D792
Water Absorption 0.080 %ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 72ISO 2039-2
Tensile Strength, Yield 60.0 MPaISO 527
Elongation at Break 25 %ASTM D638
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 2.20 GPaISO 178
Izod Impact, Notched (ISO) 0.290 J/cm²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 100 Hz
Dielectric Strength 16.0 kV/mm
@Thickness 3.17 mm
50% RH; ASTM D149
Dissipation Factor 0.0010
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 156 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CISO 75
Flammability, UL94 HB
@Thickness 0.800 mm
UL94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
Celanese Celanex® 1600A PBT, Unfilled
Celanese Celanex® 1400A PBT, Unfilled
Celanese Celanex® 1600FC PBT, Unfilled
Barlog Plastics KEBATER B510 PBT unreinforced

PHCT00 / 45640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.