MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBATER B510 PBT unreinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: PBT

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %similar to ISO 62 test
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 235 °C
20 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.0 MPa8410 psiISO 527-1
Elongation at Break >= 25 %>= 25 %ISO 527-1
Elongation at Yield 3.5 %3.5 %ISO 527-1
Tensile Modulus 2.50 GPa363 ksiISO 527-1
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 
Descriptive Properties
Resin TypePBT

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
BASF Ultradur® B 2550 PBT
Mitsubishi Chemical Advanced Materials Duratron™ D7000 PI Unfilled Polyimide

PBARLO837 / 149855

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.