MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 66GF4H Nylon 66, Conditioned, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Notes: 66GF4H is a 20% glass fiber reinforced, heat stabilized nylon 66 that offers good mechanical performance coupled with good surface finish and flow.

Availability: Europe

Fillers/Reinforcement: Glass Fiber, 20% Filler by Weight

Additive: Heat Stabilizer

Features: Good Flow; Good Surface Finish; Heat Stabilized

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Moisture Absorption at Equilibrium 2.0 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.014 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 14500 psiISO 527-2
Elongation at Break 10 %ISO 527-2
Tensile Modulus 580000 psiISO 527-2
Flexural Strength 13100 psiISO 178
Flexural Modulus 580000 psiISO 178
Izod Impact, Notched (ISO) 7.10 ft-lb/in²ISO 180/A
Charpy Impact Unnotched NBISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 518 - 554 °F
Middle Barrel Temperature 518 - 554 °F
Front Barrel Temperature 518 - 554 °F
Melt Temperature 518 - 554 °F
Mold Temperature 176 - 194 °F
Drying Temperature 176 °F
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0406 / 236897

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.