MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® 66GF4H Nylon 66, Conditioned, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Notes: 66GF4H is a 20% glass fiber reinforced, heat stabilized nylon 66 that offers good mechanical performance coupled with good surface finish and flow.

Availability: Europe

Fillers/Reinforcement: Glass Fiber, 20% Filler by Weight

Additive: Heat Stabilizer

Features: Good Flow; Good Surface Finish; Heat Stabilized

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.014 cm/cm0.0070 - 0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psiISO 527-2
Elongation at Break 10 %10 %ISO 527-2
Tensile Modulus 4.00 GPa580 ksiISO 527-2
Flexural Strength 90.3 MPa13100 psiISO 178
Flexural Modulus 4.00 GPa580 ksiISO 178
Izod Impact, Notched (ISO) 14.9 kJ/m²7.10 ft-lb/in²ISO 180/A
Charpy Impact Unnotched NBNBISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 290 °C518 - 554 °F
Middle Barrel Temperature 270 - 290 °C518 - 554 °F
Front Barrel Temperature 270 - 290 °C518 - 554 °F
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0406 / 236897

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.