MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber/MoS2 Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.22 - 1.65 g/ccAverage value: 1.42 g/cc Grade Count:43
Filler Content 10.0 - 50.0 %Average value: 31.0 % Grade Count:21
Water Absorption 0.400 - 1.30 %Average value: 0.767 % Grade Count:18
Linear Mold Shrinkage 0.00100 - 0.0150 cm/cmAverage value: 0.00467 cm/cm Grade Count:37
Linear Mold Shrinkage, Transverse 0.00500 - 0.0125 cm/cmAverage value: 0.00862 cm/cm Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118 - 121Average value: 120 Grade Count:8
Tensile Strength, Ultimate 62.1 - 228 MPaAverage value: 159 MPa Grade Count:42
Tensile Strength, Yield 125 - 125 MPa
@Temperature 90.0 - 90.0 °C
Average value: 125 MPa Grade Count:1
Elongation at Break 1.00 - 5.00 %Average value: 3.09 % Grade Count:41
Modulus of Elasticity 1.00 - 17.2 GPaAverage value: 9.74 GPa Grade Count:31
 6.70 - 6.70 GPa
@Temperature 90.0 - 90.0 °C
Average value: 6.70 GPa Grade Count:1
Flexural Yield Strength 103 - 331 MPaAverage value: 242 MPa Grade Count:40
Flexural Modulus 4.14 - 15.5 GPaAverage value: 9.22 GPa Grade Count:40
Izod Impact, Notched 0.320 - 1.71 J/cmAverage value: 0.910 J/cm Grade Count:34
Izod Impact, Unnotched 2.67 - 13.3 J/cmAverage value: 7.46 J/cm Grade Count:24
Izod Impact, Notched (ISO) 10.1 - 18.1 kJ/m²Average value: 14.1 kJ/m² Grade Count:4
Charpy Impact Unnotched 3.00 - 7.50 J/cm²Average value: 5.80 J/cm² Grade Count:5
 4.50 - 5.00 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 4.75 J/cm² Grade Count:1
Charpy Impact, Notched 0.400 - 2.30 J/cm²Average value: 1.24 J/cm² Grade Count:9
 0.800 - 0.800 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.800 J/cm² Grade Count:1
Coefficient of Friction 0.230 - 0.390Average value: 0.325 Grade Count:4
Coefficient of Friction, Static 0.180 - 0.460Average value: 0.355 Grade Count:4
K (wear) Factor 24.0 - 44.0 x 10-8 mm³/N-MAverage value: 31.0 x 10-8 mm³/N-M Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 - 1.00e+16 ohm-cmAverage value: 2.28e+15 ohm-cm Grade Count:22
 
Thermal PropertiesOriginal ValueComments
Melting Point 250 - 275 °CAverage value: 261 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 232 - 266 °CAverage value: 257 °C Grade Count:23
Deflection Temperature at 1.8 MPa (264 psi) 194 - 260 °CAverage value: 246 °C Grade Count:38
Vicat Softening Point 250 - 260 °CAverage value: 255 °C Grade Count:4
Flammability, UL94 HBGrade Count:24
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 293 °CAverage value: 281 °C Grade Count:11
Melt Temperature 270 - 310 °CAverage value: 289 °C Grade Count:25
Mold Temperature 65.6 - 120 °CAverage value: 87.7 °C Grade Count:34
Drying Temperature 79.4 - 107 °CAverage value: 84.4 °C Grade Count:25
Moisture Content 0.100 - 0.200 %Average value: 0.193 % Grade Count:15
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:14
Injection Pressure 68.9 - 124 MPaAverage value: 99.2 MPa Grade Count:23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 209 MS 1  Nylon 6/6 (PA 6/6) Glass Fiber 50% - Molybdenum Disulfide 1%
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
Overview of materials for Nylon 66, 40% Glass Fiber Filled
LATI Latilub 66-01M G/50 PA66, 50% Glass Fiber Reinforced, Molybdenum disulphide Filled
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced

O2519 / 78018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.