MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos Nova 4300 High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Features: High impact material, excellent toughness and environmental stress crack resistance, UL classification 94 HB.

Applications: Thermoformed containers and lids for the dairy industry, hot and cold beverage cups, single service packaging items

Data provided by the manufacturer.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Key Words: Nova Styrenics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 2.7 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 22.0 MPaASTM D638
Elongation at Break 65 %ASTM D638
Tensile Modulus 1.897 GPaASTM D638
Flexural Yield Strength 48.0 MPaASTM D790
Flexural Modulus 2.069 GPaASTM D790
Izod Impact, Notched 1.07 J/cmNotched; Low Orientation. ASTM D256
 1.39 J/cmNotched; High Orientation. ASTM D256
Gardner Impact 14.0 JFalling Dart Impact Injection Molded Disc, 3.2 mm x 50 mm diameter
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CASTM D648
Vicat Softening Point 97.0 °CASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 274 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Impact Modified
Tabriz HIPS 4240 High impact polystyrene
Supreme Petrochem SC 202EL General Purpose Polystyrene
Overview of materials for Polystyrene, Transparent Grade
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene

PSTN20 / 69215

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.