MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Stat-Rite® X-5076 is a static dissipative, High Impact Polystyrene alloy. Stat-Rite® X-5076 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation properties when thermoformed into complex tray designs. Gardner Drop - Impact Strength is 1.0 in-lb/mil per ASTM D-5420-93.

Features:

  • Superior static decay
  • Clean: no sloughing, low offgassing, low ionics
  • Consistent ESD properties after thermoforming
  • Carbon-free protection

Applications:

  • Electronic component packaging
  • Tape & reel
  • Component handling trays

Properties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling.

Data provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 14.5 MPa2100 psiASTM D638-95
Elongation at Break 150 %150 %ASTM D638-95
Flexural Modulus 1.10 GPa160 ksiASTM D790-95A
Izod Impact, Notched 2.14 J/cm4.00 ft-lb/inASTM D256-92
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+11 ohm-cm5.00e+11 ohm-cm50% RH; ASTM D257
Surface Resistance 5.00e+9 ohm5.00e+9 ohmESD S11.11; 50 % R.H.
Surface Resistivity per Square 5.00e+10 ohm5.00e+10 ohm50% RH; ASTM D257
Static Decay 0.30 sec0.30 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 1.5 sec1.5 secCharged Plate Monitor (+1000 V to 100 V)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 94.0 °C201 °FASTM D1525-95
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova 4300 High Impact Polystyrene
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global)
Ineos Styrenics Polystyrene 476M (NAFTA)
Celanese Celanex® 5202 PBT, 15% Glass Reinforced
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene

PNOVEON28 / 55457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.