St 7000® EHT is a further development from Wefapress, based on ultra-high molecular weight low pressure polyethylene with a molecular weight of approximately 9.2 million g/mol. This material type was finished with oxidation-inhibiting additives that allow extended use at higher temperatures.Information provided by Wefapress. |