MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wefapress St 7000® EHT PE-UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: St 7000® EHT is a further development from Wefapress, based on ultra-high molecular weight low pressure polyethylene with a molecular weight of approximately 9.2 million g/mol. This material type was finished with oxidation-inhibiting additives that allow extended use at higher temperatures.

Information provided by Wefapress.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.962 g/cc>= 0.0348 lb/in³DIN 53479
Moisture Absorption <= 0.0100 %<= 0.0100 %
Molecular Weight 9.20e+6 g/mol9.20e+6 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 65
@Time 15.0 sec
60 - 65
@Time 0.00417 hour
DIN 53505
Ball Indentation Hardness 38.0 MPa
@Time 30.0 sec
5510 psi
@Time 0.00833 hour
DIN ISO 2039 Teil 1
Tensile Strength 23.0 MPa3340 psiDIN 53455
Tensile Strength, Ultimate 35.0 MPa5080 psiDIN 53455
Elongation at Break >= 350 %>= 350 %DIN ISO / R 527
Modulus of Elasticity 0.700 GPa102 ksiDIN 53457
Charpy Impact, Notched >= 10.0 J/cm²>= 47.6 ft-lb/in²DIN 53457
Coefficient of Friction 0.120.12
Sand Slurry 8080% Abrasion
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Strength 45.0 kV/mm1140 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FDIN ISO 11359
Specific Heat Capacity 1.80 J/g-°C0.430 BTU/lb-°F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Melting Point 130 - 135 °C266 - 275 °FDTA
Maximum Service Temperature, Air 47.0 °C117 °FDimensional Stability; DIN 53461
 100 °C212 °FContinuous Application Temp.
Vicat Softening Point 80.0 °C176 °FDIN 53460
Minimum Service Temperature, Air -200 °C-328 °F
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEFA916 / 243121

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.