MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik ROHACELL® 71 HERO Aircraft Grade Polymethacrylimide (PMI) Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL® HERO is produced for composite aircraft structures that are lightweight, durable over their lifetime and less expensive to produce. HERO sandwich cores offer the most weight saving potential of all structural foams. Featuring a closed cell structure, ROHACELL® HERO minimizes added weight by taking up resin only in the cut surface cells –resulting in a lighter finished part weight compared with traditional honeycomb structures.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0750 g/ccISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 4.10 MPaISO 527-2
Elongation at Break 9.5 %ISO 527-2
Tensile Modulus 123 MPaISO 527-2
Compressive Strength 1.10 MPaISO 844
Compressive Modulus 48.0 MPaISO 844
Shear Modulus 0.0280 GPaASTM C273
Shear Strength 1.30 MPa7.2% shear strain; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 37.7 µm/m-°C
Glass Transition Temp, Tg 207 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Rohacell® 71 A Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik Rohacell® 31 A Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik ROHACELL® 200 HERO Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik ROHACELL® 51 RIMA Polymethacrylimide Foam
Evonik ROHACELL® 71 RIMA Polymethacrylimide Foam

PEVONIL307 / 196511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.