MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik ROHACELL® 71 RIMA Polymethacrylimide Foam
Categories: Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL® RIMA is a closed-cell rigid foam based on polymethacrylimide (PMI) chemistry, which does not contain any CFC's. The fine cell structure of ROHACELL® RIMA has been specially designed to ensure the minimum possible uptake of resin. This is approximately 50 g/m², which allows the end weight of the component to remain extremely low. The thermal and thermo-mechanical properties of the rigid foam are otherwise similar to those of ROHACELL® WF. ROHACELL® RIMA is particularly well suited for vacuum infusion and RTM processes, where the fine-cell foam can also be used purely as a fly-away tool. Processing is possible at a pressure of 0.7 MPa and temperatures of up to 130°C. The heat-treated material ROHACELL® RIMA-HT can be used at a temperature of 180°C and pressures of up to 0.7 MPa.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0750 g/cc0.00271 lb/in³ISO 845
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 2.20 MPa319 psiISO 527-2
Elongation at Break 7.0 %7.0 %ISO 527-2
Modulus of Elasticity 0.105 GPa15.2 ksiISO 527-2
Compressive Strength 1.70 MPa247 psiISO 844
Poissons Ratio 0.250.25Calculated
Shear Modulus 0.0420 GPa6.09 ksiASTM C273
Shear Strength 1.30 MPa189 psiASTM C273
 
Thermal PropertiesMetricEnglishComments
CTE, linear 34.0 µm/m-°C18.9 µin/in-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik ROHACELL® 71 HERO Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik ROHACELL® 51 RIMA Polymethacrylimide Foam
Evonik ROHACELL® 110 SL Polymethacrylimide Foam
Evonik ROHACELL® 51 RIST-HT Polymethacrylimide Foam
Evonik Rohacell® 71 A Aircraft Grade Polymethacrylimide (PMI) Foam

PEVONIL312 / 196516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.