MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Garlock STRESS SAVER® 6800 EPDM Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: More economical gasket where a PTFE envelope is not required.
  • Raised, molded-in sealing rings seal with 75% less surface area for high performance in non-metallic flanges
Media: Water, very mild acids and caustics

Information provided by Garlock Rubber Technologies

Key Words: ethylene propylene diene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 7060 - 70
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C
@Pressure 1.72 MPa
300 °F
@Pressure 250 psi
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
ColorOff-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock 563 EPDM Sheet Rubber
Garlock 8314 EPDM Sheet Rubber Gasketing
Garlock BLUE-GARD® 3700 Compressed Aramid Fiber Gasketing, EPDM Binder
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Garlock 567 EPDM Sheet Rubber

PGARL829 / 157512

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.