MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsance wire and cable insulation, extruded tubes. The high porosity property of this resin allows rapid plasticizer absorption reducing the compound cycle times and resulting in high compound throughput and low manufacturing cost. Geon® Atlas S140 improves heat distortion (HDT) performance, increase the strength for highly plasticized formulas, and provides longer product shelf life.

Note: The value set forth represent 'typical' values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, netweight 50lbs, 2,500lbs per pallet. Information shown on the package includes commercial identification number, lot, and weight. STP 488 (formulation): 100phr Geon® Atlas S140, 55phr TOTM, and 18phr Filler ASTM D638 (formulation): 100phr Geon® Atlas S140, 60phr DINP, 5phr ESO, and 2phr Mark 4716

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Volatiles 0.070 %0.070 %Geon® STP 793; Internal Method
Apparent Bulk Density 0.410 g/cc0.0148 lb/in³Geon® STP 1169; Internal Method
Porosity 0.57 %0.57 %cm³/g; Geon® STP 1094; Internal Method
Particle Size <= 105 µm<= 105 µm14.8%; Geon® DFT 1466; Internal Method
 145 µm145 µmAverage Particle Size Geon® DFT 1466; Internal Method
 >= 250 µm>= 250 µm3.4%; Geon® DFT 1466; Internal Method
Relative Viscosity 3.1 cP3.1 cPCorrelation, Cyclohexanone 1%; Internal Method
Viscosity Measurement 1.41.4Inherent; ASTM D1243-60-A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 17.9 MPa2600 psiOptimum; With provided formulation; ASTM D638
 
Descriptive Properties
Contamination0Internal Method; Magnetic Particles, Geon® STP 1217 Unit: #/100in2
 1Internal Method; Dark Particles, Geon® STP 1217 Unit: #/100in2
 4Internal Method; Light Colored Particles, Geon® STP 1217 Unit: #/100in2
FeaturesHigh Strength
Flow Time27 secInternal Method; Conditioned Funnel Flow Time, Geon® STP 1169
FormsPowderWhite powder
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value82Internal Method; Correlation, 0.5g/100ml
Polymerization ProcessSuspension
Powder Mix Time2.6 minInternal Method; Geon® STP 488 with provided formulation
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 1 ppmInternal Method; Geon® STP 1005
UsesInsulation
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
The Chemical Company ChemFlexx™ TOTM Trimellitate Plasticizer
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
SABIC PVC 701E Emulsion Polyvinyl Chloride for Paste Preparation
Geon® Performance Solutions FIT E 52 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

PH0POL1408 / 145977

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.