MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SABIC PVC 701E Emulsion Polyvinyl Chloride for Paste Preparation  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product Description: PVC 701E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosities at low shear rates and slightly Pseudoplastic flow characteristics at high shear rates with plasticizer concentrations of 40-60 Phr. Plastisols made from this resin exhibit the following properties:
  • Long shelf life, low viscosity aging
  • No tendency towards settling out
  • Easy gelation
  • Good thermal stability with a range of standard stabilizers
  • The potential to use high filler loadings

Typical Applications: Pastes made from PVC 701E are ideal for compact, clear thin coating, and also for chemically blown spread coatings with low plasticizer content. Applications include coatings for conveyor belts, tarpaulins, raincoats, swimming pool liners, tablecloths, wall covering, top coats, handbags, luggage, vinyl-backed carpets, and cushioned vinyl floor coverings.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.320 g/cc0.0116 lb/in³ISO 60
Volatiles <= 0.30 %<= 0.30 %ISO 1269
Particle Size <= 63 µm<= 63 µm0.75% retained; ISO 1624
 <= 106 µm<= 106 µm0.005% retained; ISO 1624
Viscosity 45000 cP
@Pressure 0.621 MPa
45000 cP
@Pressure 90.0 psi
Servers; ASTM D-1823
Brookfield Viscosity 30000 cP30000 cP20 rpm; ISO 2555/4575
 
Descriptive Properties
K-Value70ISO 1628-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Inovyn 173GB Polyvinyl Chloride Emulsion Polymer
Formosa Plastics Formolon® 113 PVC
Inovyn 172GA Polyvinyl Chloride Emulsion Polymer
Geon® Performance Solutions Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)

PSABICZ895 / 133091

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.